<?xml version="1.0" encoding="utf-8"?>
<journal>
<title>Journal of Dental Medicine</title>
<title_fa>مجله دندانپزشکی</title_fa>
<short_title>J Dent Med-tums</short_title>
<subject>Medical Sciences</subject>
<web_url>http://jdm.tums.ac.ir</web_url>
<journal_hbi_system_id>1</journal_hbi_system_id>
<journal_hbi_system_user>admin</journal_hbi_system_user>
<journal_id_issn>1024-641X</journal_id_issn>
<journal_id_issn_online>2008-2444</journal_id_issn_online>
<journal_id_pii>000</journal_id_pii>
<journal_id_doi>000</journal_id_doi>
<journal_id_iranmedex></journal_id_iranmedex>
<journal_id_magiran></journal_id_magiran>
<journal_id_sid>000</journal_id_sid>
<journal_id_nlai>000</journal_id_nlai>
<journal_id_science>000</journal_id_science>
<language>fa</language>
<pubdate>
	<type>jalali</type>
	<year>1377</year>
	<month>2</month>
	<day>1</day>
</pubdate>
<pubdate>
	<type>gregorian</type>
	<year>1998</year>
	<month>5</month>
	<day>1</day>
</pubdate>
<volume>11</volume>
<number>2</number>
<publish_type>online</publish_type>
<publish_edition>1</publish_edition>
<article_type>fulltext</article_type>
<articleset>
	<article>


	<language>fa</language>
	<article_id_doi></article_id_doi>
	<title_fa>بررسی مقاومت باند پرسلن با آلیاژهای دندانپزشکی و اثر پخت مکرر پرسلن بر آن</title_fa>
	<title>Evaluating bond strength of porcelain to dental alloys and the effects of repeated porcelain sintering on it</title>
	<subject_fa>عمومی</subject_fa>
	<subject>general</subject>
	<content_type_fa>تحقیقی</content_type_fa>
	<content_type>Research</content_type>
	<abstract_fa>&lt;font face=&quot;tahoma,arial,helvetica,sans-serif&quot;&gt;در این تحقیق مقاومت باند پرسلن، با سه نوع آلیاژ Gold-Base و Pd-Ag و Base-Metal با روش Pull-Shear مقایسه شد و اثر پخت مکرر پرسلن بر مقاومت باند مورد بررسی قرار گرفت. نتایج بدست آمده نشان داد مقاومت باند پرسلن با آلیاژ Gold-Base بیش از Pd-Ag بود و مقاومت باند آلیاژ Base-Metal در مرتبه پائین تری قرار داشت. در طی پخت مکرر پرسلن مقاومت باند در آلیاژ Base-Metal و Gold-Base تغییر معنی داری نکرد. لکن پخت مکرر پرسلن در آلیاژ Pd-Ag سبب تضعیف باند شد. &lt;/font&gt;&lt;/p&gt;                                                                  &lt;/span&gt;</abstract_fa>
	<abstract>&lt;p&gt;  In this study, porcelain bond strength to three different alloys of Gold-base, pd-Ag and base-Metal were compared and the effect of repeated porcelain sintering on bond strength was evaluated. The obtained results showed best bond strength of porcelain with Gold-base alloy. Pd-Ag and Base-metal alloys showed less strength respectively. During repeated sintering of porcelain, bond strength has not changed in Base-metal and Gold-base alloys while it was weakened in pd-Ag alloy. &lt;/p&gt;</abstract>
	<keyword_fa></keyword_fa>
	<keyword></keyword>
	<start_page>42</start_page>
	<end_page>50</end_page>
	<web_url>http://jdm.tums.ac.ir/browse.php?a_code=A-10-25-585&amp;slc_lang=fa&amp;sid=1</web_url>


<author_list>
	<author>
	<first_name>n.</first_name>
	<middle_name></middle_name>
	<last_name>Rashidan </last_name>
	<suffix></suffix>
	<first_name_fa>نیره </first_name_fa>
	<middle_name_fa></middle_name_fa>
	<last_name_fa>رشیدان</last_name_fa>
	<suffix_fa></suffix_fa>
	<email></email>
	<code></code>
	<orcid></orcid>
	<coreauthor>No</coreauthor>
	<affiliation></affiliation>
	<affiliation_fa></affiliation_fa>
	 </author>


	<author>
	<first_name>F</first_name>
	<middle_name></middle_name>
	<last_name>Geramipanah </last_name>
	<suffix></suffix>
	<first_name_fa>فریده </first_name_fa>
	<middle_name_fa></middle_name_fa>
	<last_name_fa>گرامی پناه</last_name_fa>
	<suffix_fa></suffix_fa>
	<email></email>
	<code></code>
	<orcid></orcid>
	<coreauthor>No</coreauthor>
	<affiliation></affiliation>
	<affiliation_fa></affiliation_fa>
	 </author>


</author_list>


	</article>
</articleset>
</journal>